Umutungo | Umuti ushingiye (Amavuta ashingiye) |
Umubyimba | 40mu / urwego |
Gukwirakwiza ibitekerezo | 0.2kg / ㎡ / urwego |
Gusubiramo igihe | < 2h (25 ℃) |
Igihe cyo kumisha (birakomeye) | > 24h (25 ℃) |
Ubuzima bw'umurimo | > Imyaka 15 |
Igihe cyubwubatsi | > 8 ℃ |
Shushanya amabara | Umukara |
Inzira yo gusaba | Gusasira, kuzunguruka, gukaraba |
Ububiko | 5-25 ℃, akonje, yumye |
Mbere yo kuvurwa substrate
Aluminium chlorine ya rubber primer
Chlorine rubber irwanya irangi
GusabaUmwanya | |
Birakwiye kurinda ubwato bwubwato hamwe ninyubako zimwe. | |
Amapaki | |
20kg / ingunguru. | |
Ububiko | |
Ibicuruzwa bibitswe hejuru ya 0 ℃, guhumeka neza, igicucu nahantu heza. |
Imyambarire
Usibye inyungu zayo zikora, chlorine ya rubber irwanya amarangi yubwato nayo itanga uburyo.Kuboneka mumabara atandukanye, irangi rirashobora gukoreshwa muguhuza cyangwa kuzuza ubwato bwamabara asanzwe.Ukoresheje irangi, abafite ubwato barashobora guha ubwato bwabo isura nshya mugihe bazamura imikorere.
Muri rusange, irangi rya chlorine anti-fouling irangi ni amahitamo meza kubafite ubwato bashaka kurinda ubwato bwabo no kuzamura imikorere yabo.Irangi riramba cyane, irwanya irangi, byoroshye kuyikoresha kandi iraboneka mumabara atandukanye.Hamwe nibi bintu nibyiza, ntabwo bigoye kumenya impamvu amarangi yubwato bwa chlorine anti-fouling akunzwe cyane mubafite ubwato hamwe nabakunda.
Imiterere yubwubatsi
Imiterere yubwubatsi ntigomba kuba mugihe cyizuba hamwe nubukonje (ubushyuhe ni ≥10 ℃ nubushuhe ni 85%).Igihe cyo gusaba gikurikira cyerekana ubushyuhe busanzwe muri 25 ℃.
Intambwe yo gusaba
Gutegura ubuso:
Ubuso bugomba guhanagurwa, gusanwa, ivumbi ryegeranijwe ukurikije ikibanza cyibanze;Gutegura neza substrate nibyingenzi kubikorwa byiza.Ubuso bugomba kuba bwiza, busukuye, bwumutse kandi butarangwamo uduce duto, amavuta, amavuta, nibindi byanduza.
Aluminium chlorine ya rubber primer:
1) Kuvanga (A) primer, (B) curinge agent na (C) kunanuka muri barrale ukurikije igipimo cy'uburemere;
) ;
3) Ibikoreshwa ni 0.15kg / m2.Kuzunguruka, kwoza cyangwa gutera primer kuringaniza (nkuko ishusho ifatanye yerekana) inshuro 1;
4) Tegereza nyuma yamasaha 24, intambwe ikurikira yo gusaba gutwika irangi rya chlorine anti-fouling;
5) Nyuma yamasaha 24, ukurikije uko urubuga rumeze, polishing irashobora gukorwa, ibi birashoboka;
6) Kugenzura: menya neza ko firime irangi iringaniye hamwe nibara rimwe, nta gutobora.
Rubber ya Chlorine anti-fouling coating:
)
2) Kuvanga byuzuye no kubyutsa muminota 4-5 kugeza bitarimo ibibyimba bingana, menya neza ko irangi ryuzuye;
3) Ibikoreshwa ni 0.35kg / m2.Kuzunguruka, kwoza cyangwa gutera primer kuringaniza (nkuko ishusho ifatanye yerekana) inshuro 1;
4) Ubugenzuzi: menya neza ko firime irangi iringaniye hamwe nibara rimwe, idafite umwobo.
1) Irangi ryo kuvanga rigomba gukoreshwa muminota 20;
2) Komeza icyumweru 1, urashobora gukoreshwa mugihe irangi rikomeye rwose;
3) Kurinda firime: irinde gukandagira, imvura, guhura nizuba ryizuba no gushushanya kugeza igihe firime yumye kandi igakomera.
Amakuru yavuzwe haruguru ahabwa ubumenyi bwinshi bushingiye kubizamini bya laboratoire n'uburambe bufatika.Ariko, kubera ko tudashobora guteganya cyangwa kugenzura ibintu byinshi ibicuruzwa byacu bishobora gukoreshwa, turashobora kwemeza ubwiza bwibicuruzwa ubwabyo.Dufite uburenganzira bwo guhindura amakuru yatanzwe tutabanje kubimenyeshwa.
Ubunini bufatika bwamabara burashobora gutandukana gato nuburinganire bwa theoretical twavuze haruguru bitewe nibintu byinshi nkibidukikije, uburyo bwo gukoresha, nibindi.